1. What changes between Class 1 and Class 3?
Class 1 vs Class 3 woven wire fence is mainly a coating comparison. It is not a comparison between low-carbon and high-tensile steel, or between fixed knot and hinge joint. Those choices must stay separate.
Pasture Management's published wire example lists 0.28 oz/ft² for Class 1 and 0.80 oz/ft² for Class 3. These figures show the scale of the coating difference. They are not one minimum value to apply to every diameter, standard or wire position.
| Published example | Zinc mass per surface area | Approximate metric conversion |
|---|---|---|
| Class 1 | 0.28 oz/ft² | 85.4 g/m² |
| Class 3 | 0.80 oz/ft² | 244.1 g/m² |
For those two values, 0.80 ÷ 0.28 is about 2.86. That is a coating-mass ratio, not 2.86 times the fence strength or a promise of 2.86 times its life. Check the applicable coating table for each actual wire diameter before approving an order.
2. Choose the coating for exposure and replacement cost
For a permanent farm boundary that is costly to replace, a heavier zinc coating can justify a higher purchase price. Compare Class 3 first where the project calls for it or where corrosion exposure matters. Class 1 may remain an option when the specification permits it and the buyer accepts the maintenance and replacement trade-off.
| Condition | What to compare | What the class alone cannot answer |
|---|---|---|
| Dry inland pasture | Coating premium against planned service and access | Actual life at that site |
| Salt air or industrial exposure | Heavier zinc or a separately specified alternative coating | Whether Class 3 alone meets the project requirement |
| Wet soil, manure or persistent contact | Local exposure, drainage and lower-wire protection | Underground life from an atmospheric estimate |
| Specified public or commercial work | The governing material and inspection requirements | Acceptance based on a supplier's product name |
The American Galvanizers Association identifies humidity, temperature, rainfall, pollution and salinity as relevant atmospheric factors. Its broad hot-dip galvanizing life estimates are not a warranty for a thin fence-wire coating. Likewise, South Atlantic's soil discussion depends on soil chemistry, moisture and coating thickness. Do not copy a general 20–50 year range onto a KUNYU roll.
3. Keep the standard, coating type and wire schedule together
ASTM A116-22 covers metallic-coated steel-woven fence fabric. The public scope distinguishes construction, strength grades and coating types/classes. Use the agreed edition and full requirements for acceptance; the product-page abstract is not a complete inspection specification.
State zinc versus zinc-aluminum alloy separately. Class names from different coating systems are not enough to prove equivalence. A branded zinc-aluminum coating may have its own performance evidence and warranty; those belong to that brand and product.
KUNYU's 1047-6 hinge-joint selection includes different wire packages, such as 14 ga inner wire with 12.5 ga edges and 12.5 ga inner wire with 10.5 ga edges. Keep the chosen package fixed when pricing coating options. Changing wire size at the same time prevents a clean coating comparison.
4. Verify the coating rather than judging the shine
Specify the line, edge, stay and knot wires covered by the order. Ask for batch-linked coating results using the agreed method and sampling plan. A certificate for another model or batch does not verify these rolls.
Inspect handling damage and wet packing as well as labels. A bright surface does not measure zinc mass. An instrument reading in micrometres and a mass result in g/m² also need the correct method and basis; do not treat their numbers as interchangeable.
A salt-spray result can be part of agreed testing, but it is not a direct conversion to years outdoors. The AGA explains why natural wet/dry exposure differs from that accelerated test. Keep field life, coating warranty and batch acceptance as separate claims.
5. Compare one complete quotation line
Use the same knot, full opening drawing, wire diameters, net roll length and packing for both prices. Then state only the coating difference. A 330 ft net roll is 100.584 m; do not compare it as equal to a 100 m roll without adjusting the quantity.
Send KUNYU that matched specification and quantities for FCL or LCL review. Use the wire-material comparison for the separate strength choice and the inspection checklist for batch checks.